低形宽基坩埚,可在460℃至900℃温度下进行2-5分钟的过氧化过程。
带盖 (中国进出口网)

Spun from ASTM:B551 Zirconium 702
Low-Form, wide-base crucibles can undergo 2-5 minute peroxide fusions between 460°C to 900°C.
Covers included
站内搜索/Search 手机二维码地址 随时随地,手机浏览 |
您当前的位置/Your current location:首页/Home » 进口供应/InChina » 锆坩埚Zirconium Crucibles/Covers
锆坩埚Zirconium Crucibles/Covers
详细信息/Details 原材料为ASTM:B551锆702
低形宽基坩埚,可在460℃至900℃温度下进行2-5分钟的过氧化过程。 带盖 (中国进出口网) ![]() Spun from ASTM:B551 Zirconium 702 Low-Form, wide-base crucibles can undergo 2-5 minute peroxide fusions between 460°C to 900°C. Covers included |